Liquid Oxide Dispersion Strengthened Nickel Base Superalloy

17 recipes make this.

  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    9.8 s
    Total
    23,520 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    4.9 s
    Total
    11,760 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    44.1 s
    Total
    105,840 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    1.2 s
    Total
    2,880 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    19.6 s
    Total
    47,040 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    58.8 s
    Total
    141,120 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    58.8 s
    Total
    141,120 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    4.9 s
    Total
    11,760 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    29.4 s
    Total
    70,560 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    29.4 s
    Total
    70,560 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    14.7 s
    Total
    35,280 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
  • Liquefaction FurnaceMakes Liquid Oxide Dispersion Strengthened Nickel Base SuperalloyView recipe
    MV
    Duration
    14.7 s
    Total
    35,280 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 3,960K
    • Coil: RTM Alloy
2 pages · page