Double Magnalium Plate

49 recipes use this.

  • Rotor PlatingMakes Magnalium CoatedAluminium Turbine RotorView recipe
    HV
    Duration
    30.4 s
    Total
    291,840 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • AssemblerMakes Empty Laser Cooling ContainerView recipe
    UHV
    Duration
    19 s
    Total
    437,000,000 EU
    Usage
    1,150,000 EU/t
    Conditions and notes
    • Requires Cleanroom
  • Forming PressMakes Magnalium Turbine BladeView recipe
    LV
    Duration
    20 s
    Total
    11,200 EU
    Usage
    28 EU/t
  • Liquefaction FurnaceMakes Liquid MagnaliumView recipe
    ULV
    Duration
    2.5 s
    Total
    350 EU
    Usage
    7 EU/t
    Conditions and notes
    • Temp: 800K
    • Coil: Cupronickel
  • CraftingMakes Huge Magnalium Item PipeView recipe
  • Rotor PlatingMakes Magnalium CoatedAmprosium Turbine RotorView recipe
    HV
    Duration
    228.8 s
    Total
    2,196,480 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Magnalium CoatedBismuth Bronze Turbine RotorView recipe
    HV
    Duration
    56.8 s
    Total
    545,280 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Magnalium CoatedBlack Bronze Turbine RotorView recipe
    HV
    Duration
    59.2 s
    Total
    568,320 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Magnalium CoatedBrass Turbine RotorView recipe
    HV
    Duration
    45.2 s
    Total
    433,920 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Magnalium CoatedBronze Turbine RotorView recipe
    HV
    Duration
    50.4 s
    Total
    483,840 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Magnalium CoatedChromium Turbine RotorView recipe
    HV
    Duration
    40.8 s
    Total
    391,680 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Magnalium CoatedCobalt Brass Turbine RotorView recipe
    HV
    Duration
    43.2 s
    Total
    414,720 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
5 pages · page