Tungstensteel Dust

19 recipes use this.

  • Alloy Blast SmelterMakes Molten Arceusalloy2bView recipe
    ZPM
    Duration
    13,978.1 s
    Total
    34,352,578,560 EU
    Usage
    122,880 EU/t
    Conditions and notes
    • Temp: 14,200K
    • Coil: Titansteel
  • Electric Blast FurnaceMakes Hot Tungstensteel IngotView recipe
    EV
    Duration
    50 s
    Total
    1,920,000 EU
    Usage
    1,920 EU/t
    Conditions and notes
    • Temp: 3000K
    • Coil: Nichrome
  • UnpackerMakes Small Pile of Tungstensteel DustView recipe
    LV
    Duration
    0.5 s
    Total
    120 EU
    Usage
    12 EU/t
  • CentrifugeMakes Steel DustView recipe
    LV
    Duration
    17.85 s
    Total
    10,710 EU
    Usage
    30 EU/t
  • Mana InfuserMakes Mana PowderView recipe
    Duration
    1 s
    Mana Usage
    1 /t
    Total Mana
    20
  • MixerMakes HSS-G DustView recipe
    EV
    Duration
    20 s
    Total
    768,000 EU
    Usage
    1,920 EU/t
  • Alloy Blast SmelterMakes Molten Arceusalloy2bView recipe
    ZPM
    Duration
    9,365.3 s
    Total
    23,016,161,280 EU
    Usage
    122,880 EU/t
    Conditions and notes
    • Temp: 14,200K
    • Coil: Titansteel
  • Electric Blast FurnaceMakes Hot Tungstensteel IngotView recipe
    EV
    Duration
    33.5 s
    Total
    1,286,400 EU
    Usage
    1,920 EU/t
    Conditions and notes
    • Temp: 3000K
    • Coil: Nichrome
  • UnpackerMakes Tiny Pile of Tungstensteel DustView recipe
    LV
    Duration
    0.5 s
    Total
    120 EU
    Usage
    12 EU/t
  • Alloy Blast SmelterMakes Molten High Durability Compound SteelView recipe
    UV
    Duration
    1,980 s
    Total
    19,464,192,000 EU
    Usage
    491,520 EU/t
    Conditions and notes
    • Temp: 12,600K
    • Coil: Abyssalalloy
  • Alloy Blast SmelterMakes Molten High Durability Compound SteelView recipe
    UV
    Duration
    1,326.6 s
    Total
    13,041,008,640 EU
    Usage
    491,520 EU/t
    Conditions and notes
    • Temp: 12,600K
    • Coil: Abyssalalloy
  • Alloy Blast SmelterMakes Molten HSS-GView recipe
    EV
    Duration
    438.75 s
    Total
    16,848,000 EU
    Usage
    1,920 EU/t
    Conditions and notes
    • Temp: 4,200K
    • Coil: RTM Alloy
2 pages · page