Double Chromium Plate

49 recipes use this.

  • Rotor PlatingMakes Chromium CoatedAluminium Turbine RotorView recipe
    HV
    Duration
    52 s
    Total
    499,200 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Assembly LineMakes Super Blast SmelterView recipe
    UHV
    Duration
    60 s
    Total
    2,359,296,000 EU
    Usage
    1,966,080 EU/t
    Conditions and notes
  • Forming PressMakes Chromium Turbine BladeView recipe
    MV
    Duration
    41.6 s
    Total
    99,840 EU
    Usage
    120 EU/t
  • Liquefaction FurnaceMakes Liquid ChromiumView recipe
    LV
    Duration
    5.2 s
    Total
    3,120 EU
    Usage
    30 EU/t
    Conditions and notes
    • Temp: 1,020K
    • Coil: Cupronickel
  • CraftingMakes Huge Chromium Fluid PipeView recipe
  • Rotor PlatingMakes Chromium CoatedAmprosium Turbine RotorView recipe
    HV
    Duration
    250.4 s
    Total
    2,403,840 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Chromium CoatedBismuth Bronze Turbine RotorView recipe
    HV
    Duration
    78.4 s
    Total
    752,640 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Chromium CoatedBlack Bronze Turbine RotorView recipe
    HV
    Duration
    80.8 s
    Total
    775,680 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Chromium CoatedBrass Turbine RotorView recipe
    HV
    Duration
    66.8 s
    Total
    641,280 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Chromium CoatedBronze Turbine RotorView recipe
    HV
    Duration
    72 s
    Total
    691,200 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Chromium CoatedCobalt Brass Turbine RotorView recipe
    HV
    Duration
    64.8 s
    Total
    622,080 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
  • Rotor PlatingMakes Chromium CoatedElementium Turbine RotorView recipe
    HV
    Duration
    94.4 s
    Total
    906,240 EU
    Usage
    480 EU/t
    Conditions and notes
    • Half-reaction charge: -2
    • Electrolyte system: Aqueous
5 pages · page