Beryllium Aluminum Z Ring

7 recipes use this.

Voltage
  • Liquefaction FurnaceMakes Liquid Beryllium Aluminum ZView recipe
    MV
    Duration
    0.2 s
    Total
    480 EU
    Usage
    120 EU/t
    Conditions and notes
    • Temp: 2,186K
    • Coil: Kanthal
  • Item TagsMakes Aluminium RingView recipe
  • TagsMakes Adamantium RingView recipe
  • Plasma ScrappingTakes apart Beryllium Aluminum Z RingView recipe
    LV
    Duration
    0.15 s
    Total
    90 EU
    Usage
    30 EU/t
  • Part GrindingTakes apart Beryllium Aluminum Z RingView recipe
    LV
    Duration
    0.2 s
    Total
    128 EU
    Usage
    32 EU/t
  • Data ScanningMakes Beryllium Aluminum Z RingView recipe
    432432
  • Item TagsMakes Beryllium Aluminum Z RingView recipe