Hot Aluminum Alloy 8090 Ingot
gtocore:hot_aluminum_alloy_8090_ingot, from GTOCore
2 recipes make this.
- HV
- Duration
- 55 s
- Total
- 528,000 EU
- Usage
- 480 EU/t
Conditions and notes- Temp: 1760K
- Coil: Cupronickel
- HV
- Duration
- 36.85 s
- Total
- 353,760 EU
- Usage
- 480 EU/t
Conditions and notes- Temp: 1760K
- Coil: Cupronickel